Usage Method - 1:
1. By usage of spraying “Metal Degreasing Cleaner”to clean the grease or dirty metal surface.
2. Fresh water clean after the Cleaner spray cleaning, allow the surface to dry before make-up spray again.
3. Component (A+B) Application:
(1) Remove Component A white color cover, plug-in Red color trigger head piece to the pressurized Component A can top.
(2) Open Component B cover, remove the bottle opening sealing gasket (aluminum foil type). Screw in the cover to component B bottle again. Open the Component B cover center small hole, insert the plastic capillary tubing through the center hole to Component B bottle.
(3) Insert the capillary tubing extruded end to the Red trigger head underside. Then connect by turning tight in the Component B bottle to the Red Trigger head, The Components “A+B” is combined together ready to spray.
(4) after make-up spraying, coating will be dry within 5 minutes, Allow coating to fully dry and consolidate for 24 hours (ambient temperature of 25°C).